Polymer Property : Flexural Yield Strength = 6900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 47.6 - 117 MPa
6900 - 17000 psi
Average value: 76.5 MPa Grade Count:43
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Flexural Yield Strength 47.6 MPa
6900 psi
ASTM D790
Ineos ABS Lustran® 356 Extrusion, Low-Gloss  (discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with