Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 44.8 - 55.2 MPa | 6500 - 8000 psi | Average value: 49.6 MPa Grade Count:5 |
Overview of materials for Nylon 11 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Yield Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Spartech Sound X Noise Abatement Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 44.8 MPa | 6500 psi | ASTM D790 |
PlastxWorld CEVIAN® A1300 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |