Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 42.1 MPa | 6100 psi | ASTM D790 |
Techmer ES Statiblend® PP FR BK Availability: North AmericaForms: PelletsFeature: Flame Retardant, Homopolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |