Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 3.92 - 131 MPa | 569 - 19000 psi | Average value: 47.4 MPa Grade Count:273 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 3.92 MPa | 569 psi | ASTM D638 |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Flexural Yield Strength | 3.92 MPa | 569 psi | ASTM D790 |
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided .. |
|||
Flexural Yield Strength | 3.92 MPa | 569 psi | ASTM D638 |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Flexural Yield Strength | 3.92 MPa | 569 psi | ASTM D790 |
Total PSI 4440(AS) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |