Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.3 MPa @Thickness 3.20 mm |
5400 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 37.3 MPa @Thickness 6.40 mm |
5400 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 37.3 MPa @Thickness 6.40 mm |
5400 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5204H PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 37.3 MPa @Thickness 6.40 mm |
5400 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5204S PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Eastman Tenite Butyrate 530A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9086 (FDA Odor Mask), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |