Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 42800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 295 MPa
42800 psi
ASTM Data
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
Flexural Yield Strength 295 MPa
42800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RX02059 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX02059 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include; Internally Lubricated.