Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 29.5 MPa | 4280 psi | Test specimens were injection molded by ASTM D1897; ASTM D790 |
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is eas.. |
|||
Flexural Yield Strength | 29.5 MPa | 4280 psi | ASTM D790 |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Flexural Yield Strength | 29.5 MPa | 4280 psi | ASTM D790 |
Tipco Tipcolene® FX 6000 - UL94-V0 Flame Retardant & Mineral Reinforced Polypropylene Copolymer Mineral Reinforced V0 Flame Retardant PP CopolymerApplications: Modular SwitchesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,