Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced |
|||
Flexural Yield Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Flexural Yield Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-01027 A 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |