Polymer Property : Flexural Yield Strength = 3050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 21.0 MPa
3050 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Europe-Africa-Middle East)
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE.
Flexural Yield Strength 21.0 - 47.0 MPa
3050 - 6820 psi
Average value: 38.2 MPa Grade Count:9
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Flexural Yield Strength 21.0 - 48.0 MPa
3050 - 6960 psi
Average value: 36.6 MPa Grade Count:10
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..
Flexural Yield Strength 21.0 - 51.7 MPa
3050 - 7500 psi
Average value: 42.2 MPa Grade Count:17
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..