Polymer Property : Flexural Yield Strength = 270000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 1860 MPa

@Temperature 25.0 °C
270000 psi

@Temperature 77.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Information provided by HexCel