Mechanical Properties Metric English Comments
Flexural Yield Strength 181 - 181 MPa

@Temperature 232 - 232 °C
26300 - 26300 psi

@Temperature 450 - 450 °F
Average value: 181 MPa Grade Count:1
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Yield Strength 181 MPa

@Thickness 3.20 mm
26300 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® GP2300R PBT+GF30%
Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
Flexural Yield Strength 181 MPa

@Thickness 3.20 mm
26300 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® SG5300 PBT+PET+GF30%
Description: Injection Molding, PBT+PET+GF30%, Good Surface Application: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
Flexural Yield Strength 181 MPa
26300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl PX7446 PPE+PS
This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 181 MPa
26300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE.
Flexural Yield Strength 181 MPa
26300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing Glass Fiber.
Flexural Yield Strength 181 MPa
26300 psi
ASTM D790
Cheng Yu Plastic ML3435 PC, 35% Glass Fiber
Flexural Yield Strength 181 MPa
26300 psi
ASTM D790
Cheng Yu Plastic T883GV25 Flame Retardant PBT, 25% Glass Fiber
Flexural Yield Strength 181 MPa
26300 psi
ASTM D790
Cheng Yu Plastic T889G25 PBT, 25% Glass Fiber
Flexural Yield Strength 181 MPa
26300 psi
ASTM D790
Cheng Yu Plastic FV30730 POM, 30% Mineral Reinforced