Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 1034 MPa @Temperature 23.0 °C |
150000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Flexural Yield Strength | 1034 MPa @Temperature 23.0 °C |
150000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M60J Fiber Information provided by HexCel |
|||
Flexural Yield Strength | 1030 MPa @Temperature 25.0 °C |
150000 psi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |