Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 88.2529 - 88.3 MPa @Temperature 149 - 150 °C |
12800.0 - 12800 psi @Temperature 300 - 302 °F |
Average value: 88.3 MPa Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Unfilled |