Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 48.0 - 255 MPa | 6960 - 37000 psi | Average value: 84.2 MPa Grade Count:104 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Flexural Yield Strength | 121 - 255 MPa | 17500 - 37000 psi | Average value: 181 MPa Grade Count:55 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 138 - 255 MPa | 20000 - 37000 psi | Average value: 217 MPa Grade Count:19 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Flexural Yield Strength | 71.0 - 255 MPa | 10300 - 37000 psi | Average value: 130 MPa Grade Count:176 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Yield Strength | 80.0 - 255 MPa | 11600 - 37000 psi | Average value: 141 MPa Grade Count:28 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Flexural Yield Strength | 65.5 - 255 MPa | 9500 - 37000 psi | Average value: 138 MPa Grade Count:19 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Flexural Yield Strength | 214 - 255 MPa | 31000 - 37000 psi | Average value: 241 MPa Grade Count:3 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Flexural Yield Strength | 55.2 - 255 MPa | 8000 - 37000 psi | Average value: 165 MPa Grade Count:51 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |