Polymer Property : Flexural Yield Strength = 220 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 95.0 - 220 MPa
13800 - 31900 psi
Average value: 167 MPa Grade Count:81
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Flexural Yield Strength 110 - 220 MPa
16000 - 31900 psi
Average value: 155 MPa Grade Count:21
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Flexural Yield Strength 74.5 - 220 MPa
10800 - 31900 psi
Average value: 151 MPa Grade Count:46
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Flexural Yield Strength 31.0 - 220 MPa
4500 - 31900 psi
Average value: 77.7 MPa Grade Count:74
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..