Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 83.0 - 166 MPa | 12000 - 24100 psi | Average value: 109 MPa Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |