Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 56.0 - 159 MPa | 8120 - 23000 psi | Average value: 88.2 MPa Grade Count:49 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 105 - 159 MPa | 15200 - 23000 psi | Average value: 142 MPa Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Flexural Yield Strength | 8.20 - 159 MPa | 1190 - 23100 psi | Average value: 88.9 MPa Grade Count:669 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Yield Strength | 29.1 - 159 MPa | 4220 - 23100 psi | Average value: 81.1 MPa Grade Count:304 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |