Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 7.35 - 103 MPa | 1070 - 15000 psi | Average value: 75.3 MPa Grade Count:57 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 72.0 - 103 MPa | 10400 - 15000 psi | Average value: 89.2 MPa Grade Count:24 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Yield Strength | 24.0 - 103 MPa | 3480 - 15000 psi | Average value: 82.9 MPa Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Flexural Yield Strength | 86.2 - 103 MPa | 12500 - 15000 psi | Average value: 91.6 MPa Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 2.83 - 103 MPa | 410 - 15000 psi | Average value: 74.9 MPa Grade Count:45 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Yield Strength | 38.0 - 103 MPa | 5510 - 15000 psi | Average value: 57.6 MPa Grade Count:19 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |