Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 45.5 - 221 MPa | 6600 - 32000 psi | Average value: 172 MPa Grade Count:42 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | |
Spartech Royalstatâ„¢ R671 ABS Static Control Sheet Data provided by the manufacturer. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 45.5 MPa | 6600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |