Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 294 MPa | 42700 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN133G43SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 294 MPa @Thickness 3.20 mm |
42700 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 294 MPa | 42700 psi | DIN 53455; ASTM D790 |
Kolon KOPEL® KP3363 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Flexural Yield Strength | 294 MPa | 42600 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Flexural Yield Strength | 294 MPa | 42700 psi | ASTM D790 |
Cheng Yu Plastic NG1600S Nylon 66, 60% Glass Fiber Reinforced |
|||
Flexural Yield Strength | 294 MPa | 42600 psi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Flexural Yield Strength | 294 MPa | 42600 psi | ASTM D790 |
Plenco 50045 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |