Mechanical Properties Metric English Comments
Flexural Yield Strength 24.1 - 207 MPa
3500 - 30000 psi
Average value: 150 MPa Grade Count:55
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Flexural Yield Strength 24.1 MPa
3500 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 24.1 MPa
3500 psi
ASTM D790
Westlake Plastics Kynar® 1000HD PVDF Homopolymer
Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab..
Flexural Yield Strength 24.1 MPa
3500 psi
ASTM D790
Westlake Plastics PEEK
PEEK is a high performance semi-crystalline thermoplastic. PEEK characteristics include high temperature performance, excellent wear properties, superior chemical resistance and outstanding toughne..
Flexural Yield Strength 24.1 MPa
3500 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 24.1 MPa
3500 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 24.1 MPa
3500 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Copyright © lookpolymers.com All Rights Reserved