Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 22.0 MPa | 3190 psi | ASTM D790 |
NYCOA 2011 Copolymer Nylon impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 22.0 - 393 MPa | 3190 - 57000 psi | Average value: 206 MPa Grade Count:148 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Flexural Yield Strength | 22.0 - 65.0 MPa | 3190 - 9430 psi | Average value: 42.9 MPa Grade Count:15 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |