Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 164.8 MPa | 23900 psi | ASTM D790 |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 164.8 MPa | 23900 psi | ASTM D790 |
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |