Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ASTM D882
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ASTM D882
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Borealis FS1560 High Density Polyethylene
FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Total PPH 6088 Polypropylene Homopolymer, Cast Film
Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Borealis FS1470 High Density Polyethylene
FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ASTM D882
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ASTM D882
Eastman GSP01 Copolyester for Film and Sheet Extrusion
Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s..
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
EMS-Grivory Grivory® CF 6 S PA*
Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra..