Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can.. |
|||
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |
|||
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The.. |
|||
Film Tensile Strength at Break, TD | 40.7 MPa | 5900 psi | ASTM D882 |
NOVA Chemicals Sclair® 11H1 LLDPE Film Resin
(discontinued **) Low gel, Excellent heat sealability, Easy processability, High toughness and strengthApplications: Heavy duty sack, High strength packagingAdditives: Process stabilizer, Polymer process aid, Antiblo.. |