Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
ASTM D882
ExxonMobil Escorene® LD 712.06 Film Resin  (discontinued **)
Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular..
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
Ultimate; ASTM D882
LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica..