Polymer Property : Film Tensile Strength at Break, TD = 39900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 275 MPa
39900 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 25MB866 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use..
Film Tensile Strength at Break, TD 275 MPa
39900 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 26MB768 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi..
Film Tensile Strength at Break, TD 275 MPa
39900 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 30MB666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Film Tensile Strength at Break, TD 275 MPa
39900 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 30MBR666 OPP Film
Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist..
Film Tensile Strength at Break, TD 275 MPa
39900 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 32MB768 OPP Film
Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu..
Film Tensile Strength at Break, TD 275 MPa
39900 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 30LL666 OPP Film
Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..