Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 142 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 200 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 48 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 500 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 75 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Break, TD | 211 MPa | 30600 psi | 50% RH; Strain rate 50%/min; ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 92 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |