Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 85 AXT OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 18 MAT OPP Film Product Description: Bicor MAT is a one-side matte finish, one-side treated, non-heat sealable OPP film designed for use as the outer web of a lamination. MAT is also an excellent matte finish slip .. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 70 CSR-M OPP Film Product Description: Bicor CSR-M is a one-side matte finish, on-side treated, non-heat sealable OPP film designed for cold seal release as the outer web of a lamination. CSR-M is also an excellent m.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 514P Polyester Film This high clarity film has one side hydrophilic pretreated to promote adhesion to many solvent coatings formulations, while the opposite side is pretreated to provide antistatic protection.Informati.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 690 Polyester Film, 142 Gauge Melinex® 690 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge Melinex® 965 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 400 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 500 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 750 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 1000 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 275 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 400 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 500 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 650 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 700 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 750 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO Polyester Film, 500 Gauge Product Description: Mylar® MO polyester film has excellent electrical properties. This film offer exceptional cut-through resistance, low shrinkage, low moisture absorption, and high thermal durab.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 70 HBS-2 OPP Film Product Description: Bicor HBS-2 is a one-side sealable, one-side high barrier PVdC-coated OPP film designed for use as the inside sealant web in high-barrier laminations.Availability: Latin America.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 943 Polyester Film Melinex® 943 is a super clear film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 92 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 500 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WC Polyester Film, 500 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 200 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 300 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Break, TD | 207 MPa | 30000 psi | ASTM D882A |
DuPont Teijin Films Mylar® S2 Polyester Film, 1000 Gauge Mylar® S2 is a slightly hazy film designed for use in the production of drumheads. It has low haze, excellent impact resistance, and balanced physical properties, resulting in consistent tonal qual.. |