Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
M. Holland Company MAGMA® LM112-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
LyondellBasell Petrothene® NA442051 Low Density Polyethylene ApplicationsPETROTHENE NA 442 is a series of low density/EVA copolymer resins for high impact/high clarity packaging and lamination applications. NA 442 exhibits excellent processability and good b.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil LDPE LD 368HD Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | |
Dow LDPE 683I Low Density Polyethylene, Film Grade DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor.. |
|||
Film Tensile Strength at Break, TD | 19.3 MPa | 2800 psi | ASTM D882 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |