Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 49.70 MPa | 7208 psi | ASTM D882 |
Formosa Plastics Formolene® E927ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |