Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
SABIC F01552 High Density Polyethylene for Blown Film Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: processing aid additiveCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPEApplications: thick or t.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
Chevron Phillips Dynex™ D605A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7100 psi | ASTM D882 |
ExxonMobil Exceed™ 1327CA Blown Film Resin
(discontinued **) Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7100 psi | ASTM D882 |
ExxonMobil Enable™ 27-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Break, TD | 49.0 MPa | 7110 psi | ASTM D882 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |