Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
Westlake EN1820 Low Density Polyethylene Westlake Polyethylene EN1820 natural is a low density formulation with outstanding optical properties, making this material an excellent choice for calendaring and as a clarity filler in coextruded .. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3310 psi | |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Film Tensile Strength at Break, TD | 22.8 MPa | 3300 psi | ASTM D882 |
Dow INTEGRAL™ 899A Monolayer Adhesive Film INTEGRAL 899A Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Glass, Polyurethane Foams/Sheet, Acrylic Adhesives, Wood.. |