Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.3 MPa | 3230 psi | ASTM D882 |
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and .. |
|||
Film Tensile Strength at Break, TD | 22.3 MPa | 3240 psi | ASTM D882 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |