Polymer Property : Film Tensile Strength at Break, TD = 21.04 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 21.04 MPa
3051 psi
ASTM D882
Dow 650I Low Density Polyethylene Resin
DOW LDPE 650I Resin is intended for use in soft goods over wrap, bread bags, shrink films and other general purpose applications.Information provided by Dow