Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Eastman E6838-923F Polyethylene
(discontinued **) E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1020 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1037 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1041 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Braskem TS9022 Blown Film Extrusion Low Density Polyethylene Films for automatic overwrap packaging of hygiene markets. Typical applications are toilet tissue, kitchen paper and napkin (paper product) overwrap. Films which require good optical properties al.. |
|||
Film Tensile Strength at Break, TD | >= 18.0 MPa | >= 2610 psi | ASTM D882 |
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | 500 mm/min; ISO 527-3 |
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | 500 mm/min; ISO 527-3 |
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |