Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 3570 MPa

@Pressure 5.00 MPa,
Temperature 100 °C
518000 psi

@Pressure 725 psi,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 3570 MPa

@Pressure 10.0 MPa,
Temperature 100 °C
518000 psi

@Pressure 1450 psi,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 3570 MPa

@Pressure 15.0 MPa,
Temperature 100 °C
518000 psi

@Pressure 2180 psi,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 3570 MPa

@Pressure 20.0 MPa,
Temperature 100 °C
518000 psi

@Pressure 2900 psi,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 3570 MPa

@Pressure 25.0 MPa,
Temperature 100 °C
518000 psi

@Pressure 3630 psi,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 3570 MPa

@Pressure 30.0 MPa,
Temperature 100 °C
518000 psi

@Pressure 4350 psi,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved