Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 8210 MPa @Pressure 20.0 MPa, Temperature 23.0 °C |
1.19e+6 psi @Pressure 2900 psi, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 8180 MPa @Pressure 40.0 MPa, Temperature 23.0 °C |
1.19e+6 psi @Pressure 5800 psi, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |