Polymer Property : Dart Drop Test = 0.706 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 320 g
0.706 lb
F50; ISO 7765-1
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability..
Dart Drop Test 320 g
0.706 lb
ASTM D 1709
Total Finathene® 1288 HDPE film  (discontinued **)
Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti..
Dart Drop Test 320 g
0.706 lb
ASTM D1709
LG Chemical SEETEC ST318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica..
Dart Drop Test 320 g
0.706 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA480145 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Dart Drop Test 320 g
0.706 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA480177 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Dart Drop Test 320 g
0.706 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA480178 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Dart Drop Test 320 g
0.706 lb
ISO 7765-1
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film
Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P..
Dart Drop Test 320 g
0.706 lb
ASTM D1709A
ExxonMobil Escorene® LD 713.93 Blown Film Resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat..
Dart Drop Test 320 g
0.706 lb
ASTM D1709A
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)
Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm..
Dart Drop Test 320 g
0.706 lb
ASTM D1709
ExxonMobil Pax-Plus™ 3201 Blown Film Resin
Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista..
Dart Drop Test 320 g
0.706 lb
ASTM D1709
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati..
Dart Drop Test 320 g
0.706 lb
ASTM D1709
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati..