Polymer Property : Dart Drop Test = 0.639 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 290 g
0.639 lb
F50; ISO 7765-1
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta..
Dart Drop Test 290 g
0.639 lb
ASTM D1709
M. Holland Company MAGMA® LL1091-K LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Dart Drop Test 290 g
0.639 lb
F<sub>50</sub>; ASTM D1709A
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Dart Drop Test 290 g
0.639 lb
F<sub>50</sub>; ASTM D1709A
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Dart Drop Test 290 g
0.639 lb
F<sub>50</sub>; ASTM D1709A
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Dart Drop Test 290 g
0.639 lb
F<sub>50</sub>; ASTM D1709A
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Dart Drop Test 290 g
0.639 lb
blow ratio: 4:1, frost line: 900mm, thickness:20µm; ASTM D1709-98
Ipiranga Petrochem GM 9450 F HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Dart Drop Test 290 g
0.639 lb
D1709
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal ..
Dart Drop Test 290 g
0.639 lb
ASTM D1709
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
Notes: Terraloy™ BP-20001A is a Thermoplastic Starch/Biodegradable Copolyester ready-to-process compound that contains up to 40% of TPS renewable content and is 100% biodegradable. This compound i..
Dart Drop Test 290 g
0.639 lb
ASTM D1709
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
Dart Drop Test 290 - 1000 g
0.639 - 2.20 lb
Average value: 570 g Grade Count:12
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Dart Drop Test 290 g
0.639 lb
ASTM D1709
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr..