Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 105 g | 0.232 lb | ASTM D1709 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Dart Drop Test | 105 g | 0.232 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit.. |
|||
Dart Drop Test | 105 g | 0.232 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Dart Drop Test | 105 g | 0.232 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Dart Drop Test | 105 g | 0.232 lb | ASTM D1709A |
LyondellBasell Montell 16501F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Dart Drop Test | 105 g | 0.232 lb | ASTM D1709A |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Dart Drop Test | 105 g | 0.232 lb | ASTM D1709A |
LyondellBasell Montell 16501F6 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets .. |
|||
Dart Drop Test | 105 g | 0.232 lb | ASTM D1709A |
LyondellBasell Montell 16501F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Dart Drop Test | 105 g | 0.232 lb | ASTM D1709A |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Dart Drop Test | 105 g | 0.232 lb | |
JPJ Technologies LLD150-2 LLDPE Virgin Application: Used for ice & frozen bags, garbage bags consumer packingInformation provided by JPJ Technologies |
|||
Dart Drop Test | 105 g | 0.232 lb | F50; ASTM D1709 A |
Equate EFDA-7047 LLDPE Film Extrusion Resin EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n.. |
|||
Dart Drop Test | 105 g | 0.232 lb | F50; ASTM D1709 A |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |