Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 78.0 g | 0.172 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Dart Drop Test | 78.0 g | 0.172 lb | Method A; ASTM D1709 |
Dow 611A Low Density Polyethylene (LDPE) A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |