Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 20.0 - 350 g | 0.0441 - 0.772 lb | Average value: 200 g Grade Count:8 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |