Polymer Property : Elmendorf Tear Strength, TD = 272 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 10.7 g/micron
272 g/mil
ISO 6383-2
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film
LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o..
Elmendorf Tear Strength, TD 10.7 g/micron
272 g/mil
ISO 6383-2
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film
LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu..
Elmendorf Tear Strength, TD 10.7 g/micron
272 g/mil
ASTM D1922
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Elmendorf Tear Strength, TD 10.7 g/micron
272 g/mil
ASTM D1922
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Elmendorf Tear Strength, TD 10.7 g/micron
272 g/mil
ASTM D1922
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Copyright © lookpolymers.com All Rights Reserved