Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-0224-A LDPE
(discontinued **) Puncture value is 43.2 J/mm. LDPE. Excellent stiffness, moderate toughness, easy processability. Additive Package: Base Resin.Applications: Industrial packaging, liners, blends with LLDPE, foam art.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
Chevron Phillips MarFlex® 9608 HDPE Coating Blend Resin Resin Type: Coating Blend ResinCharacteristics: Low Gel Levels, Improves MVTR, Reduces COF, Excellent Draw Properties, Excellent Processability, Improves Scuff Resistance, Improves Stiffness Propert.. |
|||
Elmendorf Tear Strength, TD | 3.90 g/micron | 99.1 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |