Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | ASTM D1922 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | ASTM D1922 |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | ASTM D1922 |
Eastman E6838-964F Polyethylene
(discontinued **) E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Elmendorf Tear Strength, TD | 3.70 - 5.24 g/micron | 94.0 - 133 g/mil | Average value: 4.36 g/micron Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | 50 µm (2 mil) film; ASTM D1922 |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | ISO 6383-2 |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Elmendorf Tear Strength, TD | 3.70 g/micron | 94.0 g/mil | ASTM D1922 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |