Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 14.2 - 19.4 g/micron | 360 - 494 g/mil | ASTM D1922 |
BiologiQ ESR-PE EcoStarch mLLDPE Blend Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ |