Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.600 - 1.80 g/micron
15.2 - 45.7 g/mil
Average value: 1.40 g/micron Grade Count:5
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..