Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 3.27 g/micron
83.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through ..
Elmendorf Tear Strength, MD 3.27 g/micron
83.0 g/mil
ASTM D1922
Dow DOWLEX™ 2036G Linear Low Density Polyethylene
Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow