Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and.. |
|||
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and.. |
|||
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | |
Westlake Hifor SC74557 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc.. |
|||
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | |
Westlake LF2040 Hexene Linear Low Density Polyethylene Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | ASTM D1922 |
ExxonMobil EXACT™ 4150 Plastomer Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film a.. |
|||
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | ASTM D1922 |
Dow 611A Low Density Polyethylene (LDPE) A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Elmendorf Tear Strength, MD | 7.87 g/micron | 200 g/mil | ASTM D1922 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |